Title
Procena integriteta zavarenih konstrukcija projektovanih sa smanjenim stepenom sigurnosti
Creator
Jeremić, Lazar, 1991-, 64452361
Copyright date
2020
Object Links
Select license
Autorstvo-Nekomercijalno-Bez prerade 3.0 Srbija (CC BY-NC-ND 3.0)
License description
Dozvoljavate samo preuzimanje i distribuciju dela, ako/dok se pravilno naznačava ime autora, bez ikakvih promena dela i bez prava komercijalnog korišćenja dela. Ova licenca je najstroža CC licenca. Osnovni opis Licence: http://creativecommons.org/licenses/by-nc-nd/3.0/rs/deed.sr_LATN. Sadržaj ugovora u celini: http://creativecommons.org/licenses/by-nc-nd/3.0/rs/legalcode.sr-Latn
Language
Serbian
Cobiss-ID
Theses Type
Doktorska disertacija
description
Datum odbrane: 21.12.2020.
Other responsibilities
mentor
Sedmak, Aleksandar, 1955-, 12447079
član komisije
Radaković, Zoran, 1961-, 14087271
član komisije
Popović, Olivera, 1973-, 12864615
član komisije
Gnjatović, Nebojša, 1982-, 15001959
član komisije
Sedmak, Simon, 1984-, 17384039
Academic Expertise
Tehničko-tehnološke nauke
University
Univerzitet u Beogradu
Faculty
Mašinski fakultet
Alternative title
Integrity assessment of welded structures designed with reduced safety
Publisher
[L. Jeremić]
Format
[100] listova
description
Tehničke nauke – Mašinsko inženjerstvo - Tehnologija materijala / Technical Sciences – Mechanical Engineering - Materials science
Abstract (sr)
Predmet ove doktorske disertacije je istraživanje ponašanja zavarenih konstrukcija sa
smanjenim stepenom sigurnosti prema krtom lomu i otpornost na prsline u cilju ocene njenog
integriteta i veka. U tom slučaju posebna pažnja se posvećuje mestima koncentracije napona, jer se
krti lomovi ovih konstrukcija po pravilu događaju upravo na takvim mestima. Radi detaljnog
proučavanja nakstanka i rasta prsline, neophodna je primena principa mehanike loma, jer klasični
pristup konstruisanju (projektovanju) preko faktora koncentracije napona i čvrstoće u tom slučaju
nije dovoljan. Primenom parametra mehanike loma, kao što je faktor inteziteta napona, čiji opseg
definiše brzinu rasta prline, a čija kritična veličina (žilavost loma) određuje kritičnu dužinu prsline.
Time se obezbeđuje pouzdana procena integriteta konstrukcije (ako se dokaže da je faktor
intenziteta napona manji od žilavosti loma), odnosno procena veka konstrukcije (primenom zakona
mehanike loma na izračuvavanje krritičnih parametara za poznatu ili pretpostavljenu početnu
dužinu prsline, njenu kritičnu vrednost, kao i izračunati opseg faktora intenzitata napona).
Konzervativni pristup u svim koracima ove procedure obezbeđuje pouzdanu eksploataciju
konstrukcije sa smanjenim stepenom sigurnosti.
Abstract (en)
The subject of this doctoral dissertation is the research of the behavior of welded structures
with a reduced degree of safety on brittle fracture and crack resistance in order to assess its integrity
and age. In this case, special attention is paid to the stress concentration points, since the fractures
of these structures tend to occur exactly in such places. For the detailed study of the crack and
growth of the crack, it is necessary to apply the principle of fracture mechanics, since the classical
approach to design (design) through the factor of stress concentration and strength is not sufficient
in that case. Using the fracture mechanics parameter, such as the voltage intensity factor, whose
range defines the rate of crack growth, and whose critical size (fracture toughness) determines the
critical crack length. This ensures a reliable assessment of the integrity of the structure (if it is
proven that the stress intensity factor is less than the tensile strength of the fracture), or the
assessment of the century of construction (by applying laws of fracture mechanics to calculate
critical parameters for known or assumed initial crack length, its critical value, as well as calculate
the range voltage intensities factor). A conservative approach in all steps of this procedure ensures
reliable exploitation of a structure with a reduced degree of safety
Authors Key words
Integritet, zavarena konstrukcija, cevovod, čelik povišene čvrstoće SM80P, mehanika loma
Authors Key words
Integrity, welded construction, pentock, steel of high strength SM80P, fracture mechanics
Classification
539.42:621.791.05(043.3)
Type
Tekst
Abstract (sr)
Predmet ove doktorske disertacije je istraživanje ponašanja zavarenih konstrukcija sa
smanjenim stepenom sigurnosti prema krtom lomu i otpornost na prsline u cilju ocene njenog
integriteta i veka. U tom slučaju posebna pažnja se posvećuje mestima koncentracije napona, jer se
krti lomovi ovih konstrukcija po pravilu događaju upravo na takvim mestima. Radi detaljnog
proučavanja nakstanka i rasta prsline, neophodna je primena principa mehanike loma, jer klasični
pristup konstruisanju (projektovanju) preko faktora koncentracije napona i čvrstoće u tom slučaju
nije dovoljan. Primenom parametra mehanike loma, kao što je faktor inteziteta napona, čiji opseg
definiše brzinu rasta prline, a čija kritična veličina (žilavost loma) određuje kritičnu dužinu prsline.
Time se obezbeđuje pouzdana procena integriteta konstrukcije (ako se dokaže da je faktor
intenziteta napona manji od žilavosti loma), odnosno procena veka konstrukcije (primenom zakona
mehanike loma na izračuvavanje krritičnih parametara za poznatu ili pretpostavljenu početnu
dužinu prsline, njenu kritičnu vrednost, kao i izračunati opseg faktora intenzitata napona).
Konzervativni pristup u svim koracima ove procedure obezbeđuje pouzdanu eksploataciju
konstrukcije sa smanjenim stepenom sigurnosti.
“Data exchange” service offers individual users metadata transfer in several different formats. Citation formats are offered for transfers in texts as for the transfer into internet pages. Citation formats include permanent links that guarantee access to cited sources. For use are commonly structured metadata schemes : Dublin Core xml and ETUB-MS xml, local adaptation of international ETD-MS scheme intended for use in academic documents.